Abstract

This study quantitatively determined the extraction of lead from CRT funnel glass and examined the mechanisms of thermally reducing lead in the products of sintering Pb-glass with carbon in the pre-heated furnace. The experimentally derived results indicate that a 90.3 wt% lead extraction efficiency can be achieved with 20 wt% of C addition at 950 °C for 3 min under air. The formation of viscous semi-liquid glass blocked the oxygen supply between the interaction of C and Pb-glass, and was highly effective for the extraction of metallic Pb. A maximum of 87.3% lead recover was obtained with a C to Na2CO3 ratio of 1/3 at 1200 °C. The decrease of C/Na2CO3 ratio enhanced the metallic lead recovery by increasing the glass viscosity for effective sedimentation of metallic lead in the bottom. However, with the further increase of temperature and treatment time, re-vitrification of lead back to silicate-glass matrix was detected in both Pb-glass/C and Pb-glass/C/Na2CO3 systems. The findings indicated that with proper controls, using C as an inexpensive reagent can effectively reduce treatment time and energy, which is crucial to a waste-to-resource technology for economically recovering lead from the waste CRT glass.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.