Abstract

The spent catalyst from vinyl acetate synthesis contains large quantity of zinc. The present study attempts to leach zinc using a mixture of ammonia, ammonium carbonate and water solution, after microwave treatment. The effect of important parameters such as leaching time, liquid/solid ratio and the ammonia concentration was investigated and the process conditions were optimized using surface response methodology (RSM) based on central composite design (CCD). The optimum condition for leaching of zinc from spent catalyst was identified to be a leaching time of 2.50 h, a liquid/solid ratio of 6 and ammonia concentration 5.37 mol/L. A maximum of 97% of zinc was recovered under the optimum experimental conditions. The proposed model equation using RSM has shown good agreement with the experimental data, with a correlation coefficient ( R 2) of 0.95. The samples were characterized before and after leaching using X-ray diffraction (XRD), nitrogen adsorption and scanning electron microscope (SEM).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.