The lateritic nickel ore sample subjected to this experimental study was taken from Karacam ore deposit (Eskisehir-Turkey) and contains 1.80% Ni, 23.90% Fe, 1.58% Mg and 0.034% Co. According to the mineralogical analysis of lateritic nickel ore samples, goethite, hematite, wustite, retgersite, gaspeite, quartz and clay type minerals were observed. The leaching conditions of lateritic nickel ore in a nitric acid medium were investigated by studying the effects of its leaching parameters, such as stirring speed, temperature, nitric acid concentration and the particle size of the sample on Ni extraction. The maximum nickel extraction was obtained with the following conditions: 200 rpm stirring speed, 10/500 g/mL solid/liquid ratio, 240 min of leaching time, a 2.0 M nitric acid concentration, 80°C leaching temperature and -38 μm particle size fraction.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.