Abstract
This paper discusses the leaching behavior of simulated high-level-waste cabal glass (CaO–B 2O 3–Al 2O 3) as a bulk specimen. During leach tests, the glass is immersed in either deionized water or in groundwater for up to 57 days at 70°C. Based on the results, mechanisms observed with the leaching of the glass in deionized water or groundwater are discussed. Three factors, i.e., time of immersion, type of leaching solution and irradiation effect, are extensively studied. The corrosion was found to be linear with time in the limit of investigation (1–57 days) but with different rates depending on the type of solution and glass composition. Effects of γ-irradiation on the glass together with groundwater were found to decrease the glass durability. The evolution of the damage on mechanical and physical properties of the glass before and after leaching or irradiation was also discussed. The addition of waste oxide changes the properties of the glass matrix, so the influence of the guest oxides on the properties of host materials is also discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.