Abstract
Phonon densities of states (DOS) for the high performing thermoelectric material, AgPbmSbTe2+m (LAST-m, m = 16, 18, and 20), were extracted from time-of-flight inelastic neutron scattering measurements. The phonon DOS of LAST-18 differs remarkably from LAST-16 and LAST-20 by exhibiting a dramatic broadening of its acoustic modes that increases on heating. This broadening coincides with a minimum in the thermal conductivity, a maximum in the electrical conductivity and Seebeck coefficient, and a related peak in thermoelectric performance. We argue that the anomalous broadening originates with scattering enhanced by modifications to Te-Ag(Sb) bonds caused by their resonant electronic states falling near the Fermi energy for m = 18.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.