Abstract

Dry films formed by surfactant-stabilized, peroxide-initiated styrene–butyl acrylate latex were examined by atomic and electric force microscopy (AFM and EFM). The effects of latex serum components on the films were observed by subjecting the latex to extensive dialysis prior to film formation, and comparing the results to as-prepared latex. The films formed with the dialyzed latex are smoother (as evidenced by roughness and fractal dimension measurements) than the films from the as-prepared latex, but they display large electric force gradients between neighboring domains. The films made with the as-prepared latex have the highest electric uniformity, with a maximum potential variation lower than 80 mV, while this reaches 200 mV in the dialyzed latex film.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.