Chemical etching of single-crystalline (100)Si induced by pulsed laser irradiation at 308, 423, and 583 nm has been investigated as a function of the laser fluence and C12 pressure. Without laser-induced surface melting, etching requires Cl radicals which are produced only at laser wavelengths below 500 nm. With low laser fluences (Φ(308 nm) 440 mJ/cm2) etching is thermally activated. In the intermediate region both thermal and non-thermal mechanisms contribute to the etch rate.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.