Al2O3−34 wt.% TiC ceramics have been machined with a KrF (248 nm) excimer laser under normal atmosphere. In the initial steps of the irradiation process both the roughness and the removal rate present a strong variation with the number of pulses. After approximately 200 pulses the process reaches a stationary regime where the roughness and the removal rate become constant. Characterization of the machined areas by scanning electron microscopy showed that the variations in roughness and removal rate are related to the evolution of the surface topography of the samples. Also, as a consequence of laser irradiation, TiC and Al2O3 are partially transformed into TiO2, TiC0.7N0.3, and an Al–Ti solid solution.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.