Aluminum-magnesium-scandium-zirconium (AlMgScZr) alloys need to be rapidly cooled from the liquid state to obtain a high degree of solute supersaturation that helps to exploit the precipitation hardening potential of the material. While AlMgScZr alloys have been successfully used in laser powder bed fusion (LPBF) processes, there has been little research in the field of laser directed energy deposition (DED) of the material. The limited previous studies have shown that the performance of AlMgScZr parts fabricated with DED only reached about 60% of that of the parts fabricated with LPBF. In view of breaking through the limitation associated with the process conditions of conventional DED, this work demonstrates the DED of AlMgScZr alloys in high-speed process regimes and elucidates the mechanism of enhancing the hardness and tensile strength of AlMgScZr alloys by increasing the cooling rate by one to two orders of magnitudes, as well as reducing the track overlapping and the porosity of the specimens during the process. A maximum average hardness of nearly 150 HV0.1 and a max. tensile strength of 407 MPa are obtained by using an energy per unit length of 5400 J/m and a powder feed rate per unit length of 0.25 g/m.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.