Abstract
AbstractTransient electronics that can chemically or physically disappear after a period of stable operation have been achieved through various metal and semiconductor materials. Despite excellent properties and wide availability of 2D materials and van der Waals (vdW) thin‐film electronics, transient films and devices based on them have rarely been reported, not to mention large‐area production with high throughput. Here, a photonic sintering approach is developed to achieve large‐area transient vdW films that may be used for bioresorbable devices. The approach can process 2D materials such as graphite, graphene, and transition metal sulfide, resulting in continuous films that are 10 × 10 cm2 in area and ≈60 to ≈440 nm in thickness on transient substrates. The influence of interfacial adhesion and sintering conditions to the thickness and the electrical properties of transient graphite films is investigated. In addition, the transient films can yield conductive patterns such as biopotential electrodes, interdigital electrodes, and resistor arrays using complementary metal–oxide–semiconductor (CMOS) fabrication processes or a two‐step sintering method. The photonic sintering method may eventually lead to large‐area transient electronics for innovative applications in healthcare, data security, and consumer electronics, and enrich the category of transient electronics through achievement of more printable transient vdW electronics.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.