Abstract
Anti-sintering Pd/TiO2 catalysts have been prepared by different methods and systematically characterized. Compared with the catalysts prepared by the heterogeneous deposition precipitation (HDP) method and wetness impregnation (WI) method, the catalyst prepared by the deposition precipitation (DP) method could give higher content of Pd species. Pd/TiO2 prepared by DP method shows much higher activity than other catalysts in liquid phase oxidation of benzyl alcohol to benzyl aldehyde. The average particle size of Pd nanoparticles (NPs) is 15nm. XPS results indicate that though Pd2+ species have been reduced to Pd0 after use, the activity of catalyst is not affected, which has never been reported in the literature.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.