Carbon nanotubes (CNTs) were prepared through catalytic pyrolysis of phenol resin at 600°C under Ar atmosphere using ferric nitrate as the catalyst precursor. The structure and morphology of pyrolyzed resin were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The results show that the optimum growth temperature of the CNTs is 600°C, and other heating temperatures lower or higher than 600°C are not suitable for large-scale preparation of CNTs. Moreover, the ferric nitrate experienced the following phase transformation: Fe3O4 at 400°C, catalytically active Fe at 600°C and catalytically inactive (Fe, C) carbide at 800 and 1000°C. Based on the SEM and TEM results, a four-step mode of Vapour-solid-solid (VSS) and tip growth mechanism was revealed for the formation of CNTs from catalytic pyrolysis of phenol resin.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.