Abstract

Single crystals of LnBS3 (Ln = La–Nd) were synthesized by the combined boron–chalcogen mixture and molten flux growth methods. SHG measurements confirmed the expectation that LaBS3 would exhibit a strong SHG response, measured at 1.5 × KDP.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.