Abstract

This paper is devoted to the fabrication of laminated Ti3SiC2/Zr based composites from Ti3SiC2 filled preceramic paper and Zr powder. The composites represented a “layers-by-layer” structure and were sintered by spark plasma at 1400 °C and 50 MPa for 10-30 min. The densification behavior during the sintering, microstructure of obtained composites and influence of the holding time on the phase composition were studied.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.