Abstract

This paper conveys the laboratory investigation of the storage stability of CRM binder as a basic study. The CRM binder was produced through the wet process in the laboratory. The percentages of crumb rubber used for rubberized binder were 5%, 10%, 15% and 20%. The samples were prepared according to ASTM D7173. In order to evaluate the properties of each part of the binders, tests were carried out through the rotational viscosity and viscoelasticity, and the separation index was assessed with the G*/sin δ and %rec. In general, the results of this study revealed that (1) the conditioned CRM binders appeared to have higher viscosity in the bottom part compared to the middle and top parts.; (2) similar to the viscosity results, the CRM binders after conditioning showed the highest G*/sin δ value in the bottom part; (3) from the MSCR test, Jnr and % rec values are observed to have a similar trend with G*/sin δ results, although some of the data were not measured due to the higher load than the DSR test; and (4) it was discovered that the SI from G*/sin δ generally used was suitable for evaluating the storage stability of CRM asphalt binders, compared to the SI from % rec.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call