Abstract

This paper aims at investigating some physical and mechanical characteristics of cemented tailings paste incorporating different amounts of crushed waste rocks (hereinafter called paste aggregate fill, PAF) for underground stope filling. Different mixture formulations were prepared with three classes of crushed waste rocks (or aggregate) grain size, namely 0/10, 0/15 and 0/20 mm. The amount of crushed waste rocks in the PAF mixtures ranges from 10 to 50% by volume (% v/v) (or 8–45% by mass, %m) of dry mill tailings and crushed waste rocks. The results show that the addition of crushed waste rocks in cemented tailings paste mixtures allows a significant unconfined compressive strength (UCS) development after 28 and 90 days of curing. The highest UCS was obtained from the mixtures containing 50% v/v of crushed waste rocks of class of size 0/15 mm. The PAF mixtures with the coarser crushed waste rocks (class of size of 0/20 mm) exhibit some particles segregation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.