Abstract

La 0.75Sr 0.25Cr 0.5Mn 0.5O 3 (LSCM) has been applied as hydrogen electrode (cathode) material in solid oxide electrolysis cells operating with different steam concentrations (20, 40, 60 and 80 vol.% absolute humidity (AH)) using 40 sccm H 2 carrier gas at 800, 850 and 900 °C, respectively. Impedance spectra and voltage–current curves were measured as a function of cell electrolysis current density and steam concentration to characterize the cell performance. The cell resistance decreased with the increase in electrolysis current density while increased with the increase in steam concentration under the same electrolysis current density. At 1.6 V applied electrolysis voltage, the maximum consumed current density increased from 431 mA cm −2 for 20 vol.% AH to 593 mA cm −2 for 80 vol.% AH at 850 °C. Polarization and impedance spectra experiments revealed that LSCM–YSZ hydrogen electrode played a major role in the electrolysis reaction.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.