Abstract

Polycrystalline alumina specimens with and without MgO doping show smoothly curved grain boundaries after heat treatment at 1400°C indicating their rough structure. When heat-treated at 1400° and 1500°C for 24 h after packing in an alumina–YAG powder mixture, many grain boundaries (without any liquid phase) develop kinks of large and small scales as observed by scanning electron microscopy and transmission electron microscopy. The addition of Y2O3 at concentrations close to the solubility limit is thus shown to induce the grain boundary transition to singular structures.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.