Abstract
As one of the top ten on nickel laterite ore resources in the world, Indonesia must have been initiating the nickel processing in total amount of about 1.5 million tonnes. In regard to the low nickel laterite processing, one of the possible product is nickel pig iron (NPI) needed for the stainless steel industries. In this study carbon raiser that is waste from oil industries was used to replace metalurgical coke. The kinetic of nickel laterite reduction using carbon raiser was studied and compared with anthrasite coal. In this work, the author conducted the reduction of nickel laterite ores by both carbon raiser and anthrasite coal as reductant, in air and CO2 atmosphere, within the temperature ranged from 800°C and 1000°C. Two models were applied, sphere particle geometry model and Ginstling-Brounhstein diffusion model, to study the kinetic parameters. The results indicated that type of reductants and reduction atmosphere greatly influence the kinetic parameters. The obtained values of activation energy were varied between 17.44-18.12 kcal/mol.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.