Abstract
Three magnetic hard alloys 22Kh15K, 25Kh15KYuBF and 30Kh5K of the Fe-Cr-Co system are used to study the kinetics of σ phase formation after quenching from 1300–1100°C and tempering in the temperature range 700–800°C by measuring HV300 hardness, X-ray diffraction, and metallographic analysis. The main σ-forming element in these alloys is shown to be cobalt. The rate of formation of σ-phase during tempering is maximal at 750°C.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.