The kinetics of gas phase hydrogen uptake into platinized VMoO5.5 to form the bronze H−3.2VMoO5.5 is limited by diffusion of atomic hydrogen from Pt crystallites to the mixed oxide (spillover). It is therefore strongly dependent on the precursor platinum salt (H2PtCl6, Pt(NH3)4Cl2 or Pt(NH3)4(OH)2) as well as on the pretreatment conditions between salt deposition and hydrogen exposure, since these parameters determine platinum dispersion. While traditional techniques for metal dispersion measurement, such as CO adsorption or H2 adsorption/titration are inappropriate for this system, semi-quantitative information on Pt dispersion can be extracted from a simple analysis of the kinetics. These dispersion estimates are in reasonably good agreement with average particle sizes obtained from TEM micrographs.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.