Abstract
The study of the return to equilibrium state of PbCdBiSn and PbCdBiMg alloys has been studied. Indeed, two structural states were considered: raw casting alloy and rehomogenized alloy. The experimental temperatures are 20°C and 80°C. The latter temperature was selected because it corresponds to the temperature of ripening of battery grids and extreme temperature for operating a battery. We studied the kinetics of Pb2%Cd1%Bi0,5%Sn and Pb2%Cd1%Bi2%Mg. The activation energy of the alloy without tin remains less than the one with tin and approximate to that with Magnesium.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Letters of Chemistry, Physics and Astronomy
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.