A kinetic modeling of the hydrogen interaction with a Pd-SiO2-Si (Pd-MOS) device is reported. The model is fitted to a number of experimental results, mainly from mass spectrometric desorption measurements. The new results verify an older description of the energetics of hydrogen adsorption states at the Pd/SiO2 interface in the sense that the adsorption may be described by a so-called Temkin isotherm; however, several new findings have to be incorporated into the model in order to obtain a consistent picture. The initial heat of adsorption at the interface is around 0.8 eV/hydrogen atom. The number of adsorption sites at the interface is considerably smaller than at the surface, 6×1017 m−2 versus 1.5×1019 m−2. Furthermore, the interface hydrogen atoms are strongly polarized. An average value of 2 Debye is obtained. It is the large hydrogen polarization at the Pd/SiO2 interface and not a large concentration of adsorbed hydrogen atoms per se which accounts for the very high sensitivity of a Pd-MOS device as hydrogen sensor.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.