Abstract
Copper-chromite active metal catalyst was prepared by using impregnation method with kieselguhr (Al2O3SiO2) as supporting material. The content of metal active was 20% with 1:1 proportion of complex metal Cu : Cr. The specific surface area of catalyst gave specific surface area of 2,537 m2/ gram. X-ray Diffraction analysis, shown that active metal of Cu-copper Cu and cristobalite SiO2. Temperature program analysis, shown that reduction temperature of catalyst was 300 0Cusing by Scanning Electronic Microscope (SEM), the morphology of catalyst was determined.Keyword : Copper-Chromite catalyst, impregnation, Kieselguhr
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.