Abstract
Electrical explosion of wire has a prosperous future in fine powder producing. In the process of electrical explosion of segmented metal wire (EESW),energy deposited in the wire was influenced by process variables such as the initial charging voltage of the capacitors, the length and the diameter of the segmented wire,and the electrode spacing. For understanding their relation completely, a series of experiments of electrical explosion was carried out with variations of the initial charging voltage and the segmented wire lengths and diameter. Results show that, energy deposition efficiency was weakly dependent on the wire length , whereas it has a strong dependence on the wire diameter, the initial charging voltage of the capacitors have an important influence on the energy deposition.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.