Abstract
Parameters of the non-Debye relaxation in the 10Sc1CeSZ solid electrolyte made of various types of ZrO2 powder stabilized with 10-mol.% Sc2O3 and 1-mol.% CeO2 were studied. The influence of powder properties and their sintering temperatures on the impedance spectra is analyzed. In regard to electrical response, the polycrystalline ceramic electrolytes may be considered as a single-phase or a two-phase material consisting of a grain bulk and a boundary. In many cases, the boundary resistance is independent practically on dopants and their distribution across the powders and sintering temperatures. The powder compositions suitable for an electrolyte and electrodes are specified.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.