To develop the new bonding method under low bonding temperature and short holding duration, pulse electric current sintering (PECS) method is applied. The Ni plating layer was used as the interlayer. The following experimental factors were researched:(1) Thickness of Ni plating layer, (2) Bonding temperature, (3) Bonding pressure and (4) Heat treatment after plating. The bonding strength of W-Ni plate-Cu joint could be obtained under low bonding temperature of 773 K and short bonding duration of 10 min.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.