JIc tests using the multiple specimen procedure described in ASTM standard E813 were conducted at room temperature and −45°C (−50°F) with five common carbon or low alloy cast steels, viz., 0030, 0050A, C-Mn, Mn-Mo, and 8630. Specimen thickness was 25.4 mm (1 in.). Valid JIc values were obtained with four of the cast steels at room temperature and only two of the cast steels at −45°C (−50°F). Only Jcl (Jcleavage) values were obtained with the four other tests due to unstable brittle or cleavage fracture. Valid JIc values were obtained if the test temperature was above the mid-point temperature of the Charpy V notch energy transition region as measured along the temperature axis. Conservative estimates of KIc were calculated from JIc test results and a preliminary empirical equation involving KIc and Sy at room temperature and upper shelf CVN energy was suggested for cast steels. Room temperature JIc values were higher for the three tempered martensitic cast steels than for the two ferritic-pearlitic cast steels.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.