Abstract
Open-cell porous aluminum (Al) was fabricated by friction powder sintering (FPS) process without using external heat sources. In this process, powder mixture of Al powder and sodium chloride (NaCl) powder as spacer particle was used as starting material. The compacting and sintering of the mixture were conducted only by rotating tool plunged into a die and mixture. NaCl was removed by placing the sintered mixture in water. In this study, porous Al was fabricated using ADC6 powder, and pore structures of obtained porous Al were nondestructively observed by X-ray CT. In addition, compression properties of obtained porous Al were investigated.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: The Proceedings of Mechanical Engineering Congress, Japan
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.