Increased joint laxity is associated with excessive polyethylene wear, but the correlation between laxity and metal wear has not been established. Fifteen necropsy-retrieved primary total knee replacements were mounted into a custom knee-testing machine that measured anterior-posterior, varus-valgus, and internal-external rotational laxity at 0°, 30°, 60°, and 90° of flexion. Inductively coupled plasma-mass spectrometry analysis was performed to measure the cobalt (Co), chromium (Cr), and titanium (Ti) concentrations in periprosthetic tissue samples. Spearman's rank correlations were performed to determine whether a significant correlation (p < 0.05) existed between soft tissue laxity and tissue metal concentrations. At 0° flexion, decreased posterior displacement was negatively correlated with elevated Co and Cr concentrations. At 30° flexion, decreased external rotation and varus deflection was negatively correlated with elevated Ti concentrations. At 60° flexion, decreased anterior displacement was negatively correlated with elevated Cr concentrations and decreased varus deflection was negatively correlated with increased Ti concentrations. At 90° flexion, decreased anterior displacement was negatively correlated with elevated Co and Cr concentrations. To our knowledge, this is the first study to investigate the correlation between tissue metal concentration and laxity. Decreased laxity was associated with elevated metal concentrations in periprosthetic tissue.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.