Abstract

The influence of gaseous KCl on the high temperature oxidation of CrMoV11 1 (X20) steel at 600degreesC is reported. The sample temperature was above the dew point of KCl, the partial pressure of KCl being about 5ppm. The samples were investigated by a number of surface analytical techniques including grazing angle XRD, SEM/EDX, and SAM. CrMoV11 1 steel shows protective behaviour in clean dry O-2 and O-2/H2O environment because of the formation of a chromium-rich oxide (alpha-(Fe,Cr)(2)O-3). It is Often considered that alkali salts accelerate the corrosion of steel only when present on the surface in solid or liquid form. In contrast, the present result shows that gaseous KCl is very corrosive, also in the absence of condensation. KCl(g) reacts with chromium in the scale, forming K2CrO4(s). This depletes the protective oxide in chromium and leads to the formation of non-protective hematite, Fe2O3.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.