AbstractWe have directly measured the solubility of iron and nickel in high and low boron-doped silicon using Instrumental Neutron Activation Analysis. Boron doping levels were 1.5×1019 and 6.5× 1014 atoms/cm3. Iron and nickel impurity concentrations were measured after extended indiffusions at 800, 900, 1000 and 1100°C for iron and 600, 700 and 800°C for nickel. We have measured a significant enhancement of Fe and Ni concentrations in high boron-doped silicon as compared to low boron-doped silicon. Based on these measurements, we show the iron donor energy level shifts towards the valence band with increased temperature, e.g. at 900°C the donor level is 0.24eV above the valence band as opposed to 0.39eV at room temperature. These results demonstrate that the impurity energy level shift with temperature must be accounted for in any prediction of segregation gettering of metal impurities into heavily doped substrates and heavily implanted doping layers. Additionally, our results suggest that either Ni solubility is greatly enhanced and/or the Ni diffusivity is greatly decreased with high boron doping of silicon.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.