Abstract
We compared the ionic properties of yttria-stabilized zirconia (YSZ) thin films prepared by atomic layer deposition (ALD) using various oxidants including water, oxygen, and ozone. Cross-plane conductivity measurements were performed at low temperature (50°C) and high temperature (450°C) using AC impedance spectroscopy. As a result, we have confirmed that the conductivity of ALD YSZ films below 300°C is greater by several orders of magnitude compared to the nano-scale YSZ thin films synthesized by other conventional techniques. Among the ALD YSZ samples, ALD YSZ fabricated using water showed the highest conductivity while ALD YSZ fabricated using ozone showed the lowest. We have analyzed this result in relation with grain morphology characterized by X-ray diffraction (XRD) and atomic force microscopy (AFM), and the chemical binding states measured by X-ray photoelectron spectroscopy (XPS).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Similar Papers
More From: Thin Solid Films
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.