LDPE/P4VP films synthesized by in situ sorption and thermal polymerization of 4-vinylpyridine, (4VP), were used for conductivity investigations. The conductivities of swollen films varied from 7×10−6 to 1.21×10−3 S.cm−1 at room temperature depending on P4VP mass increase in the host matrix. For the temperature range of 303–333K the conductivity varied from 7×10−6 to 2.66×10−3 S.cm−1. A comparison between Arrhenius and VTF plots for conductivity measurements showed a best fit for temperature dependence according Arrhenius modified equation. The materials are stable for temperatures below 645 K.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.