The ionic electrical conduction in sintered Bi2O3-Y2O3 system for samples containing 20-30 mol% Y2O3 was investigated by means of measurement of ac conductivity and the emf of oxygen gas concentration cell using the specimen tablet as electrolyte. The experimental po2 range from 1 to 10-21 atm for ionic electrical conduction measurement-These materials showed high oxygen ionic conduction, the conductivities for samples containing 22.5-30mol% Y2O3 are many times higher than those of stabilized zirconia ZrO based solid electrolyte at corresponding temperatures. When these materials are used to construct an oxygen concentration cell, the E/E0 is equal to 1 or approaches 1. These values show that the samples containing 22.5 to 30 mol% Y2O3 are nearly pure ionic conductors. The p-type hole conductivity is very small at higher po2 values, so it is negligible. The n-type electronic conduction was investigated by means of coulomb titration technique for Y2O3 27.5 mol% sample We obtained that lg pe'=-767000/T +665. The pe' is equal to 2.6×10-61 atm at 800℃. The n-type electronic conduction is vary small, so that it is also negligible.These materials are proved to be good high ionic conductors.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call