Abstract

AlN and GaN thin films were deposited by plasma-enhanced atomic layer deposition using trimethylmetal precursors. The films were found to have high oxygen incorporation, which was attributed to oxygen contamination related to the plasma system. The choice of nitrogen containing plasma gas (N2, N2/H2 or NH3) determined the severity of oxygen incorporation into deposited films. Lowest oxygen concentrations were attained for AlN and GaN thin films using NH3 and N2 plasma, respectively. Initial experiments have shown that GaN thin films with low impurity concentrations can be deposited when plasma-related oxygen contamination is avoided by the use of an alternative plasma source.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.