Abstract

The thermal atomic layer deposition (ALD) of tungsten-rich tungsten carbide thin films is described using WCl6 and the aluminum dihydride co-reactant AlH2(tBuNCH2CH2NMe2). Smooth and stable films were grown at temperatures >200 °C. An ALD window was observed between 275-350 °C with a growth rate of 1.6 Å/cycle, according to SEM and XRR. Self-limiting growth was demonstrated at 300 °C for both precursors. XPS analysis showed that high purity tungsten-rich tungsten carbide (WxC, x = 2.8-3.7) films were deposited at 300 °C, with low levels of nitrogen (< 4 at.%), oxygen (< 4 at.%), chlorine (< 3 at.%), and aluminum (< 1 at.%). The as-deposited films were nanocrystalline and converted to the non-stoichiometric β-WC1-x phase above 600 °C. Film densities of the as-deposited films according to XRR were 50-60% of bulk values, which may explain the relatively high film resistivities (1140 mΩ·cm at 300 °C) despite the high film purity.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.