Abstract
The mechanical properties of cured wood adhesive films were tested in a dry state by means of nanoindentation. These studies have found that the application of adhesives have an effect on the accuracy of the hardness and elastic modulus determination. The highest values of hardness among the tested adhesives at 20 °C have condensation resins: MF (0.64 GPa) and RPF (0.52 GPa). Then the decreasing EPI (0.43 GPa), PUR (0.23 GPa) and PVAc (0.14 GPa) adhesives. The values of the elastic modulus look a little bit different. The highest values among the tested adhesives at 20 °C have EPI (11.97 GPa), followed by MF (10.54 GPa), RPF (7.98 GPa), PVAc (4.71 GPa) and PUR (3.37 GPa). X-ray micro-computed tomography was used to evaluate the adhesive joint by the determination of the voids. It has been proven that this value depends on the type of adhesive, glue quantity and reactivity. The highest values of the void ratio achieve the PUR (17.26%) adhesives, then PVAc (13.97%), RRF (6.88%), MF (1.78%) and EPI (0.03%). The ratio of the gaps increases with the higher joint thickness. A too high proportion of voids may weaken the adhesive joint.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.