Abstract

In the previous articles concerning the treatment of poly(tetrafluoroethylene) (PTFE) with potassium permanganate/nitric acid mixture, the conversion of a hydrophobic to a hydrophilic surface was partially assigned to the defluorination of PTFE and then the introduction of carbonyl and hydroxyl groups into the defluorinated sites. In the present work, PTFE sheets were treated with potassium permanganate/nitric acid, and the surfaces before and after treatment were comparatively characterized by Fourier transform infrared spectroscopy (FTIR), X-ray photoelectron spectroscopy (XPS), X-ray diffraction (XRD) and scanning electron microscopy (SEM). The surface sediments of the treated PTFE were also determined by atomic absorption spectroscopy (AAS). The results indicate that the conversion of the hydrophobicity to the hydrophilicity on the modified PTFE surface is mainly due to the deposition of hydrophilic manganese oxides which covered the fluorocarbon surface, and no detectable chemical reactions of PTFE occur in the treating process.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.