Abstract

In this study, certain technological variants of the laser welding of alloy 1424 of the Al–Mg–Li–Zr system are considered with the purpose of obtaining the durability level of the welded joint, which is close to that of the basic metal. It is shown that, in the case of using various types of plastic deformation of the welded joint, its durability can be increased considerably to 0.85–0.95 from that of the basic metal.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.