Abstract
AbstractHyaluronic acid (HA) has been crosslinked in solution with glutaraldehyde (GTA), 1‐ethyl‐3‐(3‐dimethylaminopropyl) carbodiimide (EDC), poly(ethylene glycol) diglycidylether (EX 810), and divinyl sulfone (DVS) to form hydrogels. Flory‐Rehner calculations were used to determine molecular weight between crosslinks (Mc), the crosslink density (Ve), and mesh size (ε) of crosslinked hydrogels after 24‐h swelling in distilled water. Generally, lower molecular weight films gave rise to decreased molecular weights between crosslinks as well as increased effective crosslink densities and decreased mesh size. The effects of pH and salt concentration were evaluated. Use of lower molecular weight HA gave rise to decreased molecular weights between crosslinks as well as increased effective crosslink densities and decreased mesh size. Water diffusion coefficients were measured for DVS and GTA hydrogels and were found to be 1.4 × 10−10 and 1.8 × 10−10 m2 s−1. Autocrosslinked and HA polyethyleneimine gels were also produced but had very limited stabilities compared with the covalently crosslinked materials. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2008
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.