The surface properties of commercial TiO2 and samples synthesized by the thermal decomposition procedure using several precursor salts were investigated by a microelectrophoresis technique. The iep was determined as a function of the ionic strength which was controlled with KNO3 or KCl. The experimental results showed: 1) The commercial sample and the ones synthesized from the chloride salt dissolved in HCl 1:1 (v/v) show low iep’s due to chloride inclusion; 2) The purification methods explored (oxide suspension at pH~12 and dialysis) are inefficient; 3) TiO2 samples synthesized from an organic precursor salt under totally chloride-free conditions furnished an iep of 5.9 in excellent agreement with literature data; 4) Chloride specific adsorption on TiO2 is weak.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.