Magnesium phosphate ceramics are a class of acid–base cements for bioengineering and civil engineering applications. We report on quasielastic neutron scattering results focusing on the evolution of the state of water in the system during the setting reaction, to shed light on the reaction mechanisms and the nature of the products. In the first few minutes, a consistent fraction of water molecules appears as immobile, and after a transient time, they start to be progressively bound into a reaction product. The kinetics of this last process has been described with an equation combining an Avrami model and a first-order reaction model with apparent activation energies of 18 and 6 kJ/mol, respectively. The results indicate that during the reaction the water molecules experience confinement effects inside a restricted space. The size of the confining volume decreases as the reaction progresses. It is proposed that an amorphous precursor with high surface area, bonding a relevant fraction of water, but also ho...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.