Abstract

Tantalum Carbide (TaC) reinforcement was made to lamellar graphite (gray) cast irons that were produced in the physical conditions of a foundry at reinforcement ratios of 0%, 0.025%, 0.155%, and 0.285%. Samples complying with standards were prepared using the TaC-reinforced lamellar graphite (gray) cast iron alloys that were produced, and Brinell hardness tests, compressive strength tests, and microstructural analyses were conducted. According to the test results, the highest average Brinell hardness value was found as 231 HB in sample A which was reinforced at a ratio of 0.025%. In general, as the reinforcement ratio increased, there was an increase in the hardness test measurement results. The highest average compressive strength value was found as 949 MPa in sample C which was reinforced at a ratio of 0.285%. In general, as the reinforcement ratio increased, there was an increase in the compressive strength values. The results of the microstructural analyses showed that the reinforcement material was dispersed into the matrix.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.