The quantum of work with silicon carbide (SiC) and zirconium dioxide (ZrO2) in the aluminum hybrid composite material has increased due to the growing demand for lightweight materials for various industrial applications. The aluminum hybrid composite with the wt% of primary reinforcement particles of SiC was kept constant at 5%, and the secondary reinforcement particles of ZrO2 were taken by 5%, 10%, and 15%. The sintering parameters were used as the temperature at 600°C, holding time of 35 minutes, and pressure at 30MPa. In this work, the aluminum composite material reinforced with 5%wt of SiC particles compared the test results with aluminum hybrid composite reinforcement of SiC and ZrO2 nanoparticles. Adding ZrO2 reinforcements enhances the aluminum hybrid composite material's better microstructure, microhardness, tensile strength, compression, and yield strength.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.