Abstract

Bonding technology namely as “sew free” technology is usually applied for joining the pieces of sportswear and leisure clothing. Influence of the thermal ageing duration on the peeling strength of woven fabric and knitted materials bonded at 150°C temperature for 10 s, 20 s, 30 s, and 40 s durations with two polyurethane films of 0.175 mm and 0.127 mm thicknesses has been investigated in this research. Based on the research results it was shown that the peeling strength of the textile bonds is dependent on material type and bonding duration, but it is not highly affected by the ageing at 45°C temperature for 150 min, 300 min, and 450 min. During concluding it may be stated that ageing at 45°C temperatures is not main factor influencing the bond quality during its exploitation in high temperature environment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.