Abstract

A laboratory metallurgical analysis of head-hardened rails, removed from a heavy haul site at various stages of life, has enabled a study to be made of the incidence of rolling contact fatigue cracks and the role played by the white etching layer. It is shown that the cracks occurring down the center of the rail are associated with white etching layer formed very early on in the life of the rail. As the traffic carried accumulated, the extent of the white layer and the population of cracks were reduced as the white layer was removed by a spalling wear mechanism. Some of the cracks penetrated beyond the white layer-pearlite interface and grew to a depth that was not always removed during normal rail maintenance grinding. These observations would explain why some head-hardened rails have had to be removed from track after only 200 million gross tons of traffic as a result of severe spalling to a depth of 3 mm.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.