Abstract
We report an experimental investigation of the pits formed at oxidation. The pits were formed by a long time oxidation in a dry or wet atmosphere at high temperature (~ 1200 oC). Although they were observed in (0001) face, they were not in (000-1) face. Comparing the points of oxidation pits to those of molten KOH etching pits on the same area of the substrate, we show that the oxidation pits are formed by oxidizing defects. In addition, the influence of the oxidation pits to the reliability of thermal oxide was researched.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.