Abstract
Linear friction welding (LFW) method is a solid-state manufacturing process. In the present study, GH4169 superalloy was welded using LFW method. Macro morphology and shortening of LFW GH4169 joints were investigated to understand the effect of welding variables on the geometric parameters such as joint shape and size. Detailed microstructural and mechanical property of the welded GH4169 material were investigated to understand the effect of welding variables on the microstructure as well as mechanical properties. Compared with the GH4169 raw material, the grains of the welded joints are refined, and the tensile strength of the joints under two sets of parameters is greater than that of the raw material.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.