In this study, the two systems of polymethylmethacrylate (PMMA) based polymer electrolyte films have been prepared by the solution casting technique. Lithium iodide (LiI) and ethylene carbonate (EC) were used as inorganic salt and plasticizer, respectively. The highest room temperature conductivity for the plasticized system and unplasticized system is 4.42 x 10-5Scm-1and 4.37 x 10-6Scm-1, respectively. The conductivity-temperature dependence studies have been performed on these films in the temperature range of 303 K to 373 K. It can be observed that the logσversus 1000/T plots obey the Arrhenius rule and VTF rule for the plasticized film and unplasticized film, respectively [1-3]. The surface morphology of the plasticized and unplasticized films was observed by using scanning electron microscope (SEM).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.